Sammanfattning
The melting behavior of the wollastonite-feldspar system was studied using high-temperature microscopy. The decrease in the silhouette area of a cylindrical sample as a function of the temperature showed behavior characteristic for each mixture. The melting behavior was expressed further as three characteristic measuring points: T1, the temperature at which the material started to sinter; T2, the temperature at which the sintering was finished; and T3, the temperature at which the material started to float out.
Originalspråk | Engelska |
---|---|
Sidor (från-till) | 167-177 |
Antal sidor | 11 |
Tidskrift | Ceramic Engineering and Science Proceedings |
Volym | 22 |
Nummer | 2 |
Status | Publicerad - 2001 |
MoE-publikationstyp | A4 Artikel i en konferenspublikation |
Evenemang | Materials and Equipment and Whitewares; A Collection Presented at the 102nd Annual Meeting of The American Ceramic Society - St. Louis, MO, USA Varaktighet: 29 apr. 2001 → 3 maj 2001 |