Laboratory studies on the ageing behaviour of waste incineration superheater ash deposits

Tutkimustuotos: LehtiartikkeliArtikkeliTieteellinenvertaisarvioitu

4 Sitaatiot (Scopus)
90 Lataukset (Pure)

Abstrakti

Combustion of biomass for heat and power generation is typically associated with the formation of highly corrosive ash deposits on heat transfer surfaces. To get a better understanding of how these deposits change in their local chemical composition and morphology with time, synthetic deposit mixtures containing different proportions of NaCl, KCl, CaCl 2, and CaO were exposed to a temperature gradient utilising a novel experimental approach. In the experiments, exposure time, steel temperature, and furnace temperature were varied. Temperature gradient induced changes in the local deposit composition, and connected to that, the deposit corrosivity were identified. Melt formed within the deposit moved toward the steel and the subsequent dissolution of formed corrosion products into the molten phase reduces its first melting temperature resulting in the direct contact between the melt and steel. CaO was shown to have a dual role in the corrosion process. CaO reacts with Cr 2O 3 and Fe 2O 3 forming CaCrO 4 and Ca 2Fe 2O 5. Especially the reaction with Cr 2O 3 destroys its protective properties toward Cl-induced corrosion. Furthermore, CaO reduces the amount of melt formed within the deposit at the prevailing temperatures, generating a porous deposit morphology enabling the diffusion of oxygen through the deposit toward the steel surface, further propagating corrosion.

AlkuperäiskieliEnglanti
Artikkeli135359
Sivumäärä9
JulkaisuEnergy
Vuosikerta320
DOI - pysyväislinkit
TilaJulkaistu - 1 huhtik. 2025
OKM-julkaisutyyppiA1 Julkaistu artikkeli, soviteltu

Rahoitus

Financial support provided by the Research Council of Finland, Decision no. 348963: \u201CInitiation and propagation of high-temperature corrosion reactions in complex oxygen-containing environments\u201D and Decision no. 338322: \u201CNew insights on the effects of temperature gradients on high temperature corrosion\u201D, and by the Swedish Cultural Foundation in Finland, Application no. 200386: \u201CForskningsprojekt om h\u00F6gtemperaturkorrosion och -kemi\u201D is highly appreciated. The authors want to thank Linus Silvander for carrying out the SEM/EDXA analyses.

YK:n kestävän kehityksen tavoitteet

Tämä tuotos edistää seuraavia kestävän kehityksen tavoitteita:

  1. SDG 12 – Vastuullinen kulutus ja tuotanto
    SDG 12 – Vastuullinen kulutus ja tuotanto

Sormenjälki

Sukella tutkimusaiheisiin 'Laboratory studies on the ageing behaviour of waste incineration superheater ash deposits'. Ne muodostavat yhdessä ainutlaatuisen sormenjäljen.

Viittausmuodot