Corrosion of super-heater steel materials under alkali salt deposits. Part 2: SEM analyses of different steel materials

BJ Skrifvars, M Westen-Karlsson, Mikko Hupa, K Salmenoja

    Tutkimustuotos: LehtiartikkeliArtikkeliTieteellinenvertaisarvioitu

    48 Sitaatiot (Scopus)

    Abstrakti

    This paper is the second in a series of two papers where we report results from laboratory-scale corrosion studies in which tailor-made well-characterized synthetic alkali salt deposits were used for corrosion testing of typical kraft recovery boiler super-heater steel materials.

    The corrosion testing was done in temperatures ranging from 450 to 600 °C. Six different alkali salts and six different steel types were used in the tests.

    In the first paper we reported generally on the corrosion tendencies of the six steels. In this second paper we continue the corrosion behavior mapping of the tested steels.

    AlkuperäiskieliEi tiedossa
    Sivut1011–1019
    Sivumäärä9
    JulkaisuCorrosion Science
    Vuosikerta52
    Numero3
    DOI - pysyväislinkit
    TilaJulkaistu - 2010
    OKM-julkaisutyyppiA1 Julkaistu artikkeli, soviteltu

    Keywords

    • Alkaline corrosion
    • High-temperature corrosion
    • Lab-scale corrosion measurements
    • Molten salts
    • SEM/EDS analyses