Combustion of biomass for heat and power generation is typically associated with the formation of highly corrosive ash deposits on heat transfer surfaces. To get a better understanding of how these deposits change in their local chemical composition and morphology with time, synthetic deposit mixtures containing different proportions of NaCl, KCl, CaCl 2, and CaO were exposed to a temperature gradient utilising a novel experimental approach. In the experiments, exposure time, steel temperature, and furnace temperature were varied. Temperature gradient induced changes in the local deposit composition, and connected to that, the deposit corrosivity were identified. Melt formed within the deposit moved toward the steel and the subsequent dissolution of formed corrosion products into the molten phase reduces its first melting temperature resulting in the direct contact between the melt and steel. CaO was shown to have a dual role in the corrosion process. CaO reacts with Cr 2O 3 and Fe 2O 3 forming CaCrO 4 and Ca 2Fe 2O 5. Especially the reaction with Cr 2O 3 destroys its protective properties toward Cl-induced corrosion. Furthermore, CaO reduces the amount of melt formed within the deposit at the prevailing temperatures, generating a porous deposit morphology enabling the diffusion of oxygen through the deposit toward the steel surface, further propagating corrosion.

Original languageEnglish
Article number135359
Number of pages9
JournalEnergy
Volume320
DOIs
Publication statusPublished - 1 Apr 2025
MoE publication typeA1 Journal article-refereed

Funding

Financial support provided by the Research Council of Finland, Decision no. 348963: \u201CInitiation and propagation of high-temperature corrosion reactions in complex oxygen-containing environments\u201D and Decision no. 338322: \u201CNew insights on the effects of temperature gradients on high temperature corrosion\u201D, and by the Swedish Cultural Foundation in Finland, Application no. 200386: \u201CForskningsprojekt om h\u00F6gtemperaturkorrosion och -kemi\u201D is highly appreciated. The authors want to thank Linus Silvander for carrying out the SEM/EDXA analyses.

UN SDGs

This output contributes to the following UN Sustainable Development Goals (SDGs)

  1. SDG 12 - Responsible Consumption and Production
    SDG 12 Responsible Consumption and Production

Fingerprint

Dive into the research topics of 'Laboratory studies on the ageing behaviour of waste incineration superheater ash deposits'. Together they form a unique fingerprint.

Cite this